[1] O. Volkova, D. Janke, Influence of the Lining on the Thermal Behaviour of a Teeming Ladle, Steel Research International 76 (2005) 313-319. https://doi.org/10.1002/srin.200506014.
[2] P.R. Scheller, Interfacial Convection and Mass Transport in Thin Liquid Layer, Steel Research International 76 (2005) 581-587. https://doi.org/10.1002/srin.200506059.
[3] S. Lachmann, J. Loh, F. Wahlers, P.R. Scheller, Reoxidation of Ni- and Ni-Fe-Alloys by Al 2 O 3 -SiO 2 Refractory Materials, Steel Research International 76 (2005) 573-580. https://doi.org/10.1002/srin.200506058.
[4] G. Gigacher, W. Krieger, P.R. Scheller, C. Thomser, Non-Metallic Inclusions in High-Manganese-Alloy Steels, Steel Research International 76 (2005) 644-649. https://doi.org/10.1002/srin.200506069.