[1] P. Scheller, R. Hagemann, Model Investigations on Slag Entrainment in Continuous Casting, Archives of Metallurgy and Materials 57 (2012). https://doi.org/10.2478/v10172-012-0024-5.

[2] S.-J. Lee, J. Mola, B.C. De Cooman, Conversion Model for the Martensitic Transformation of Banded Austenite in a Ferrite Matrix, Metall Mater Trans A 43 (2012) 4921–4925. https://doi.org/10.1007/s11661-012-1471-3.

[3] A. Kovalev, A. Jahn, A. Weiß, S. Wolf, P.R. Scheller, STT and DTT Diagrams of Austenitic Cr–Mn–Ni As-Cast Steels and Crucial Thermodynamic Aspects of γ → α′ Transformation, Steel Research International 83 (2012) 576–583. https://doi.org/10.1002/srin.201100267.

[4] J.L. Klug, R. Hagemann, N.C. Heck, A.C.F. Vilela, H.P. Heller, P.R. Scheller, Fluorine-Free Mould Powders for Slab Casting: Crystallization Control in the CaO–SiO2–TiO2–Na2O–Al2O3 System, Steel Research International 83 (2012) 1186–1193. https://doi.org/10.1002/srin.201200094.

[5] R. Hagemann, H.-P. Heller, S. Lachmann, S. Seetharaman, P.R. Scheller, Slag entrainment in continuous casting and effect of interfacial tension, Ironmaking & Steelmaking 39 (2012) 508–513. https://doi.org/10.1179/1743281212Y.0000000018.